- used for
attached displacement fixing of the truss fabric (warp knitted fabric)
- the
coating-material will be applied with the immersion or foulard
procedure on the truss fabric (warp knitted fabric)
- subsequently
with special infrared-heater tipped drying-duct,
the coated product will be dried
- working width:
213” (=5410 mm)

- approx. cycle
width: 5520 mm
- approx.
manufacturing speed: 4m/min.
- total heating
output: 310 kW
- approx.
surface temperature
at the commodity: 230° C
- the continuous
agitation provide for a homogeneous distribution of the paste
- agitator at
the paste hutch is not essential
- easy cleaning
during exchange the paste
- easy permeate
of the scrim when starting the unit
- high accuracy
in regard to the coating
- space-saving
and vertical arrangement from the heating duct
- fast warm-up
time and short cooling-off time by the drying duct
- 6 thyristor
controlled heating zones, separately adjustable
- direct
interfacing from face creation and coating
- winding and unwinding as additional intermediate stepp is not
applicable
- minor stock and drying capacity
- more economic manufacturing
- protection of
the fabric during malfunction by overheating by means of quick aeration
and cooling down of the heating duct
- dubbing with
upstream production machine and following winder system
- fabric tension
control by the pressure measurement bearing
- nominal value
regulation between coating machine and winder
- easy control
panel, which is handled by the menu
- recipe
maintenance and process visualization
|